HIPS and ABS are the first plastic materials used in household appliances, due to the high price of HIPS and ABS resin, the market has gradually developed PP(polypropylene) modified materials suitable for household appliance parts, and partially replaced HIPS and ABS resin in household appliance products with its advantages of low cost, light weight and good performance. Now the modified PP plasti...
view more
-
Why do injection molded parts develop sink marks and dimples?
2024-09-02
(1) Improper control of molding conditions If the injection pressure is too low, the injection and holding time is too short, the injection speed is too slow, the material temperature and mold temperature are too high, the cooling of the plastic part is insufficient, the temperature is too high during demolding, the temperature around the insert is too low, or there is insufficient material supply...
view more
-
(Ⅰ) How to deal with flow marks on injection-molded parts?
2024-09-27
(1) P: Poor flow of the molten material leads to the formation of concentric flow marks resembling growth rings on the surface of injection-molded parts, centered around the gate. When low-temperature, high-viscosity molten material with poor flow performance is injected into the cavity in a semi-cured, fluctuating state through the injection port and runner, the material flows along the cavity su...
view more
-
(Ⅱ) How to deal with floating fibers on injection-molded parts?
2024-09-27
Mold temperature too low Cause: If the mold temperature is too low, the melt cools too quickly during flow, causing the glass fibers to not be fully encapsulated by the base resin and float to the surface. Solution: Increase the mold temperature appropriately to ensure the melt has sufficient fluidity to uniformly coat the glass fibers. Regularly check the mold temperature control system to ensure...
view more