(Ⅱ) How to deal with floating fibers on injection-molded parts?
2024-09-27
Mold temperature too low Cause: If the mold temperature is too low, the melt cools too quickly during flow, causing the glass fibers to not be fully encapsulated by the base resin and float to the surface. Solution: Increase the mold temperature appropriately to ensure the melt has sufficient fluidity to uniformly coat the glass fibers. Regularly check the mold temperature control system to ensure...
view more
-
Tsinghua University: Study on the Comprehensive Performance and Influencing Factors of Long Glass Fiber Reinforced PA66 Composites
2024-10-22
Introduction Fiber-reinforced polymer composites, due to their lightweight and high-strength characteristics, have found applications in many fields, especially in the transportation sector, where they can effectively reduce vehicle weight and better achieve energy savings and emission reductions. Among them, long glass fiber (LGF) reinforced polyamide materials (PA/LGF) are widely used in the man...